English: Photo of a LEED pattern of a clean Platinum/Rhodium single crystal (100) (Miller index) taken in high vacuum.
日期
来源

This picture was taken with an analog camera, later digitalized with an digital camera

Previously published: Not published before 20-3-2013
作者 Mkosterv
Other information
English: Picture was taken from a LEED display in high vacuum generated by an electron gun. The diffraction spots are generated by acceleration of elastically scattered electrons onto a hemispherical fluorescent screen, a retarding field analyzer made by Riber. Taken in high vacuum using an electron gun with an energy of 85 eV. In the middle is the bright spot of the electron gun which generates the primary electron beam.]]

许可协议

我,本作品著作权人,特此采用以下许可协议发表本作品:
Creative Commons CC-Zero 本作品采用知识共享CC0 1.0 通用公有领域贡献许可协议授权。
采用本宣告发表本作品的人,已在法律允许的范围内,通过在全世界放弃其对本作品拥有的著作权法规定的所有权利(包括所有相关权利),将本作品贡献至公有领域。您可以复制、修改、传播和表演本作品,将其用于商业目的,无需要求授权。

说明

添加一行文字以描述该文件所表现的内容

此文件中描述的项目

描绘内容

ISO速度 简体中文(已转写)

80

曝光时间 简体中文(已转写)

0.005 秒钟

焦距比数 简体中文(已转写)

4.3

焦距 简体中文(已转写)

9.23 毫米

文件历史

点击某个日期/时间查看对应时刻的文件。

日期/时间缩⁠略⁠图大小用户备注
当前2013年3月20日 (三) 13:412013年3月20日 (三) 13:41版本的缩略图3,648 × 2,736(2.05 MB)Mkosterv{{subst:Upload marker added by en.wp UW}} {{Information |Description = {{en|Photo of a LEED pattern of a clean Platinum/Rhodium single crystal (100 Miller index) taken in high vacuum.}} |Source = This picture was taken with an analog camera<br/> '''Pre...